Physical

Creep Tests

ISO 899 Part 1 (1993): Plastics—Determination of Creep Behaviour—Part 1: Tensile Creep

ISO 899 Part 2 (2003): Plastics—Determination of Creep Behaviour—Part 2: Flexural Creep by Three-Point Loading

Viscosity Tests

ISO 6721 Part 10 (1997): Plastics—Determination of Dynamic Mechanical Properties—Dynamic Shear Viscosity using Parallel Plate Oscillatory Rheometer

Physical Properties - Other Tests

BS EN ISO 1183 Part 2 (2004): Plastics—Methods for Determining the Density of Non-Cellular Plastics—Part 2: Density Gradient Column Method

ISO 7387 Part 1 (1983): Adhesives with Solvents for Assembly of PVC-U Pipe Elements—Characterization—Part 1: Basic Test Methods

ISO 10363 (1992): Hot-Melt Adhesives—Determination of Thermal Stability

ISO 10364 (1993): Adhesives—Determination of Working Life (Pot Life) of Multi-Component Adhesives

BS EN ISO 11357 Part 1 (1999): Plastics—Differential Scanning Calorimetry—General Principles

ISO 11357 Part 2 (2001): Plastics—Differential Scanning Calorimetry (DSC)—Determination of glass transition temperature

ISO 11357 Part 3 (2001): Plastics—Differential Scanning Calorimetry (DSC)—Determination of temperature and enthalpy of melting and crystallisation

ISO/DIS: 11357 Part 4 (1999): Plastics—Differential Scanning Calorimetry (DSC)—Determination of Specific Heat Capacity

BS EN ISO 11357 Part 6 (2002): Plastics—Differential Scanning Calorimetry—Determination of Oxidation Induction Time

BS EN ISO 11357 Part 7 (2002): Plastics—Differential Scanning Calorimetry (DSC)—Determination of Crystallisation Kinetics

ISO/CD: 11357 Part 8 (1998): Plastics—Differential Scanning Calorimetry—Determination of Amount of Water Absorbed by Polymers

BS EN ISO 11359 Part 1 (1999): Plastics—Thermomechanical Analysis (TMA)—General Principles

BS EN ISO 11359 Part 2 (1999): Plastics—Thermomechanical Analysis (TMA)—Determination of Coefficient of Linear Thermal Expansion and Glass Transition Temperature