Mechanical

Cleavage Tests

ISO 10354 (1992): Adhesives—Characterization of Durability of Structural-Adhesive-Bonded Assemblies—Wedge Rupture Test

ISO 11343 (2003): Adhesives—Determination of Dynamic Resistance to Cleavage of High-Strength Adhesive Bonds Under Impact Conditions—Wedge Impact Method

Peel Tests

ISO 4578 (1997): Adhesives—Determination of Peel Resistance of High-Strength Adhesive Bonds—Floating-Roller Method

ISO 8510 Part 1 (1990) or BS EN 28510–1 (1993): Adhesives—Peel Test for a Flexible-Bonded-to-Rigid Test Specimen Assembly—Part 1: 90 Degree Peel

ISO 8510–2 (1990) or BS EN 28510–2 (1993): Adhesives—Peel Test for a Flexible-Bonded-to-Rigid Test Specimen Assembly—Part 2: 180 Degree Peel

ISO 11339 (2003): Adhesives—T-Peel Test for Flexible-to-Flexible Bonded Assemblies

ISO 14676 (1997)

Shear Tests

ISO 4587 (2003): Adhesives—Determination of Tensile Lap-Shear Strength of Rigid-to-Rigid Bonded Assemblies

ISO 6237 (2003): Adhesives—Wood-to-Wood Adhesive Bonds—Determination of Shear Strength by Tensile Loading

ISO 9653 (1998): Adhesives—Test method for Shear Impact Strength of Adhesive Bonds

ISO 10123 (1990): Adhesives—Determination of Shear Strength of Anaerobic Adhesives Using Pin-and-Collar Specimens

ISO 10964 (1993): Adhesives—Determination of Torque Strength of Anaerobic Adhesives on Threaded Fasteners

ISO 11003 Part 1 (2001): Adhesives—Determination of Shear Behaviour of Structural Adhesives—Part 1: Torsion Test Method Using Butt-Bonded Hollow Cylinders

ISO 11003 Part 2 (2001): Adhesives—Determination of Shear Behaviour of Structural Adhesives—Part 2: Tensile Test Method Using Thick Adherends

ISO 13445 (2003): Adhesives—Determination of Shear Strength of Adhesive Bonds between Rigid Substrates by the Block-Shear Method

Tensile Tests

BS EN ISO 527 Part 1 (1993): Plastics—Determination of Tensile Properties—General Principles

ISO 6922 (1987): Adhesives—Determination of Tensile Strength of Butt Joints

BS EN ISO 9664 (1995): Adhesives—Test Methods for Fatigue Properties of Structural Adhesives in Tensile Shear

Mechanical Properties - Other Tests

BS EN ISO 178 (1998): Plastics—Determination of Flexural Properties

ISO 604 (2002): Plastics—Determination of Compressive Properties

BS EN ISO 11403 Part 1 (2000): Plastics—Acquisition and Presentation of Comparable Multipoint Data—Part 1: Mechanical Properties