Home|Toolkits|Forums|Documents/Data|Links|About

Physical

Creep Tests

BS 5131–1.1 (1991): Methods of Test for Footwear and Footwear Materials. Adhesives. Resistance of Adhesive Joints to Heat (Creep Test)

BS 5131–1.3 (1991): Methods of Test for Footwear and Footwear Materials. Adhesives. Preparation of Test Assemblies Using Adhesives (Other than Hot Melt Adhesives) for Heat Resistance (Creep) and Peel Tests

BS 5131–1.6 (1979): Methods of Test for Footwear and Footwear Materials. Adhesives. Recommended Environmental Storage Conditions for Adhesive Joints Prior to Heat Resistance or Peeling Tests

BS 5131–1.7 (1991): Methods of Test for Footwear and Footwear Materials. Adhesives. Preparation of Test Assemblies Using Hot Melt Adhesives for Heat Resistance (Creep) and Peel Tests

BS 5350-C7 (1990): Methods of Test for Adhesives. Adhesively Bonded Joints: Mechanical Tests. Determination of Creep and Resistance to Sustained Application of Force

Viscosity Tests

Physical Properties - Other Tests

BS 5350-H2 (1982): Methods of Test for Adhesives. Physical Tests on Hot-Melt Adhesives. Determination of Low Temperature Flexibility or Cold Crack Temperature

BS 5350-H3 (1984): Methods of Test for Adhesives. Physical Tests on Hot-Melt Adhesives. Determination of Heat Resistance of Hot-Melt Adhesives

BS EN 61006 Part 0 (1993): Methods of Test for Determination of the Glass Transition Temperature of Electrical Insulating Materials