Home|Toolkits|Forums|Documents/Data|Links|About

Other

Introduction, Selection and Standard Terminology

ASTM D 907–04: Standard Terminology of Adhesives

ASTM D 6465–99: Standard Guide for Selecting Aerospace and General Purpose Adhesives and Sealants

Environmental Conditioning and Durability

ASTM D 618–00: Standard Practice for Conditioning Plastics for Testing

ASTM D 1151–00: Standard Practice for Effect of Moisture and Temperature on Adhesive Bonds

ASTM D 1183–03: Standard Practices for Resistance of Adhesives to Cyclic Laboratory Aging Conditions

ASTM D 1828–01: Standard Practice for Atmospheric Exposure of Adhesive-Bonded Joints and Structures

ASTM D 2918–99: Standard Test Method for Durability Assessment of Adhesive Joints Stressed in Peel

ASTM D 2919–01: Standard Test Method for Determining Durability of Adhesive Joints Stressed in Shear by Tension Loading

ASTM D 2295–96 (2002): Standard Test Method for Strength Properties of Adhesives in Shear by Tension Loading at Elevated Temperatures (Metal-to-Metal)

ASTM D 2557–98 (2004): Standard Test Method for Tensile-Shear Strength of Adhesives in the Subzero Temperature Range from -267.8 to -55°C (-450 to -67°F)

ASTM D 3166–99: Standard Test Method for Fatigue Properties of Adhesives in Shear by Tension Loading (Metal/Metal)

ASTM D 3762–03: Standard Test Method for Adhesive-Bonded Surface Durability of Aluminium (Wedge Test)

Surface Treatments

ASTM D 2093–03: Standard Practice for Preparation of Surfaces of Plastics Prior to Adhesive Bonding

ASTM D 2094–00; Standard Practice for Preparation of Bar and Rod Specimens for Adhesion Tests

ASTM D 2651–01: Standard Guide for Preparation of Metal Surfaces for Adhesive Bonding

ASTM D 3933–98 (2004): Standard Guide for Preparation of Aluminum Surfaces for Structural Adhesives Bonding (Phosphoric Acid Anodising)