Physical
Creep Tests
ASTM D 1780–99: Standard Practice for Conducting Creep Tests of Metal-to-Metal Adhesives
ASTM D 2293–96 (2002): Standard Test Method for Creep Properties of Adhesives in Shear by Compression Loading (Metal-to-Metal)
ASTM D 2294–96 (2002): Standard Test Method for Creep Properties of Adhesives in Shear by Tension Loading (Metal-to-Metal)
Viscosity Tests
ASTM D 562–01: Standard Test Method for Consistency of Paints Measuring Krebs Unit (KU) Viscosity Using a Stormer-Type Viscometer
ASTM D 1084–97: Standard Test Methods for Viscosity of Adhesives
ASTM D 1200–94 (1999): Standard Test Method for Viscosity by Ford Viscosity Cup
ASTM D 2556–93a (1997): Standard Test Method for Apparent Viscosity of Adhesives Having Shear-Rate-Dependent Flow Properties
ASTM D 3236–88 (2004): Standard Test Method for Apparent Viscosity of Hot Melt Adhesives and Coating Materials
Physical Properties - Other Tests
ASTM C 679–03: Standard Test Method for Tack-Free Time of Elastomeric Sealants
ASTM D 257–99: Standard Test Methods for DC Resistance or Conductance of Insulating Materials
ASTM D 523–89 (1999): Standard Test Method for Specular Gloss
ASTM D 724–99 (2003): Standard Test Method for Surface Wettability of Paper (Angle-of-Contact Method)
ASTM D 898–96: Standard Test Method for Applied Weight Per Unit Area of Dried Adhesive Solids
ASTM D 899–00: Standard Practice for Applied Weight Per Unit Area of Liquid Adhesive
ASTM D 903–00: Standard Practice for Applied Weight Per Unit Area of Liquid Adhesive
ASTM D 1005–95 (2001): Standard Test Method for Measurement of Dry-Film Thickness of Organic Coatings Using Micrometers
ASTM D 1212–91(2001): Standard Test Methods for Measurement of Wet Film Thickness of Organic Coatings
ASTM D 1337–04: Standard Practice for Storage Life of Adhesives by Viscosity and Bond Strength
ASTM D 1338–99: Standard Practice for Working Life of Liquid or Paste Adhesives by Consistency and Bond Strength
ASTM D 1400–00: Standard Test Method for Non-destructive Measurement of Dry Film Thickness of Nonconductive Coatings Applied to a Nonferrous Metal Base
ASTM D 1525–00: Standard Test Method for Vicat Softening Temperature of Plastics
ASTM D 2377–00: Standard Test Method for Tack-Free Time of Caulking Compounds and Sealants
ASTM D 2578–04a: Standard Test Method for Wetting Tension of Polyethylene and Polypropylene Films
ASTM D 2979–01: Standard Test Method for Pressure-Sensitive Tack of Adhesives Using an Inverted Probe Machine
ASTM D 3121–94(1999): Standard Test Method for Tack of Pressure-Sensitive Adhesives by Rolling Ball
ASTM D 4333–99: Test Method for the Compatibility Resistance of Mechanical Pump Dispenser Components
ASTM D 5286–01: Standard Test Methods for Determination of Transfer Efficiency Under General Production Conditions for Spray Application of Paints (V 6.02)
ASTM D 5725–99 (2003): Standard Test Method for Surface Wettability and Absorbency of Sheeted Materials Using an Automated Contact Angle Tester
ASTM D 5946–04: Standard Test Method for Corona-Treated Polymer Films Using Water Contact Angle Measurements
ASTM D 6005–03: Standard Test Method for Determining Slump Resistance of Carpet Adhesives
ASTM F 22–02: Standard Test Method for Hydrophobic Surface Films by the Water-Break Test