Home|Toolkits|Forums|Documents/Data|Links|About

ASTM STANDARDS - Number/Title

Mechanical

Cleavage Tests

ASTM D 1062–02: Standard Test Method for Cleavage Strength of Metal-to-Metal Adhesive Bonds

ASTM D 3433–99: Standard Test Method for Fracture Strength in Cleavage of Adhesives in Bonded Metal Joints

ASTM D 3807–98 (2004): Standard Test Method for Strength Properties of Adhesives in Cleavage Peel by Tension Loading (Engineering Plastics-to-Engineering Plastics)

ASTM D 5041–98 (2004): Standard Test Method for Fracture Strength in Cleavage of Adhesives in Bonded Joints

Peel Tests

ASTM D 1781–98 (2004): Standard Test Method for Climbing Drum Peel for Adhesives

ASTM D 1876–01: Standard Test Method for Peel Resistance of Adhesives (T-Peel Test)

ASTM D 3167–03a (2004): Standard Test Method for Floating Roller Peel Resistance of Adhesives

Shear Tests

ASTM D 905–03: Standard Test Method for Strength Properties of Adhesive Bonds in Shear by Compression Loading

ASTM D 1002–01: Standard Test Method for Apparent Shear Strength of Single-Lap-Joint Adhesively Bonded Metal Specimens by Tension Loading (Metal-to-Metal)

ASTM D 3044–94 (2000): Standard Test Method for Shear Modulus of Wood-Based Structural Panels

ASTM D 3163–01: Standard Test Method for Determining Strength of Adhesively Bonded Rigid Plastic Lap-Shear Joints in Shear by Tension Loading

ASTM D 3164–03: Standard Test Method for Strength Properties of Adhesively Bonded Plastic Lap-Shear Sandwich Joints in Shear by Tension Loading

ASTM D 3165–00: Standard Test Method for Strength Properties of Adhesives in Shear by Tension Loading of Single-Lap-Joint Laminated Assemblies

ASTM D 3528–96 (2002): Standard Test Method for Strength Properties of Double Lap Shear Adhesive Joints by Tension Loading

ASTM D 3983–98(2004): Standard Test Method for Measuring Strength and Shear Modulus of Nonrigid Adhesives by the Thick-Adherend Tensile-Lap Specimen

ASTM D 4562–01: Standard Test Method for Shear Strength of Adhesives Using Pin-and-Collar Specimen

ASTM D 4896–01: Standard Guide for Use of Adhesive-Bonded Single Lap-Joint Specimen Test Results

ASTM D 5379/D5379M-98: Standard Test Method for Shear Properties of Composite Materials by the V-Notched Beam Method

ASTM D 5648–01: Standard Test Method for Torque-Tension Relationship of Adhesives Used on Threaded Fasteners (Lubricity)

ASTM D 5656–04: Standard Test Method for Thick-Adherend Metal Lap-Shear Joints for Determination of the Stress-Strain Behaviour of Adhesives in Shear by Tension Loading

ASTM D 5649–01: Standard Test Method for Torque Strength of Adhesives Used on Threaded Fasteners

Tensile Tests

ASTM D 897–01: Standard Test Method for Tensile Properties of Adhesive Bonds

ASTM D 2095–96(2002): Standard Test Method for Tensile Strength of Adhesives by Means of Bar and Rod Specimens

Mechanical Properties - Other Tests

ASTM D 695–02a: Standard Test Method for Compressive Properties of Rigid Plastics

ASTM D 1995–92 (2004): Standard Test Methods for Multi-Modal Strength Testing of Autohesives (Contact Adhesives)